Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.61 cP @Temperature 25.0 °C |
0.61 cP @Temperature 77.0 °F |
|
Asahi Glass ASAHIKLIN AK-225AES Hydrochlorofluorocarbon Solvent AK-225 AES was developed as a defluxing agent. It is an azeotrope-like mixture of AK-225, ethanol and stabilizer and is suitable for use in a vapor degreaser. It effectively removes flux residues as.. |
|||
Viscosity | 0.61 cP @Temperature 25.0 °C |
0.61 cP @Temperature 77.0 °F |
|
Asahi Glass ASAHIKLIN AK-225T Hydrochlorofluorocarbon Solvent AK-225T is a mixture of AK-225, ethanol, hydrocarbon and stabilizers. This blend was developed for those customers needing a more aggressive defluxer than AK_225AES. It has proven to be effective in.. |
|||
Viscosity | 0.61 cP | 0.61 cP | |
3M Novec™ 7200 Engineered Fluid 3M™ Novec™ 7200 fluid's convenient boiling point and excellent environmental, health and safety profile make it useful as a heat transfer fluid, cleaning solvent, for lubricant deposition & many m.. |
|||
Viscosity | 0.61 cP | 0.61 cP | |
3M Novec™ 8200 Engineered Fluid 3M™ Novec™ 8200 Engineered Fluid is a clear, colorless, low-odor fluid intended to replace 1,1,1-trichloroethane and perchloroethylene in film cleaning applications.Features and Benefits:Zero ozon.. |