Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.80 - 0.84 cP | 0.80 - 0.84 cP | Intrinsic viscosity; WI No. 104 test; correlated from solution viscosity by Invista |
Invista 2201U Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |