Physical Properties Metric English Comments
Viscosity 800000 - 1.30e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
800000 - 1.30e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..