Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 125000 cP @Shear Rate 1340 1/s, Temperature 200 °C |
125000 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 360-0185 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - Non-halogen flame re.. |
|||
Viscosity | 125000 - 135000 cP @Temperature 23.0 °C |
125000 - 135000 cP @Temperature 73.4 °F |
|
Master Bond Supreme 11HT High Temperature Resistant Two Component Epoxy System Master Bond Polymer System Supreme 11HT is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room temperature. Sup.. |
|||
Viscosity | 125000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
125000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |