Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1270 cP @Temperature 25.0 °C |
1270 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 1270 cP | 1270 cP | |
Abatron AboCast/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |