Polymer Property : Viscosity = 145000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 145000 cP
145000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Viscosity 145000 cP
145000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
Viscosity 145000 cP
145000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East)
VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics.
Viscosity 145000 cP
145000 cP
Melt Viscosity, 280°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics NORYL PVX516 PPE
PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT
Viscosity 145000 cP

@Temperature 25.0 °C
145000 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Duct 2956 Low Ion Snap Cure Silver Epoxy Adhesive
TRA-DUCT 2956 is recommended for the bonding and sealing of electronic components where a combination of electrical and mechanical properties are required. This two-part, smooth, paste system of sil..
Viscosity 145000 - 195000 cP
145000 - 195000 cP
Average value: 164000 cP Grade Count:4
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..