Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 90000 - 150000 cP @Temperature 25.0 °C |
90000 - 150000 cP @Temperature 77.0 °F |
Uncured |
Permabond LH056 Anaerobic Threadsealant Permabond LH056 is a thread sealant designed for use in sealing metal pipes and fittings in sprinkler systems which may also contain CPVC piping. Permabond LH056 prevents leaks even on pipes that ar.. |
|||
Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | |
Master Bond LED401 One Component LED Curable Adhesive System Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | |
Master Bond LED403Med USP Class VI, One Component, LED Curable System Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi.. |
|||
Viscosity | 70000 - 150000 cP | 70000 - 150000 cP | |
Master Bond Supreme 3HT-80 High Strength Epoxy Adhesive Cures at 80°C Description: Master Bond Supreme 3HT-80 is a one component, heat curing epoxy system featuring excellent physical strength properties and toughness with an eye-catching curing temperature of 170-175.. |
|||
Viscosity | 80000 - 150000 cP | 80000 - 150000 cP | |
CEN® Electronic Material CTS Polyimide Resin CEN® CTS polyimide resin is a high tensile strength, thermal stable, and viscose resin solution based on aromatic polyimide. The product offers high modulus value and high dimensional stability wit.. |
|||
Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | Part A |
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |