Polymer Property : Viscosity = 16250 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 14750 - 16250 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
14750 - 16250 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2061206D1 Silver Zinc Paste
This product has been designed as a ‘one part system’ alternative to the traditional two part system, C2061103D7 (basecoat) and C2060217D3 (topcoat). It is a screen printing ink for coati..
Viscosity 14750 - 16250 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
14750 - 16250 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2100318D2 Silver Zinc Paste
This product has been designed as a ‘one part system’ alternative to the traditional two part system. It is a screen printing ink for coating barium titanate PTC ceramic substrates. Scree..