Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 17300 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
17300 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT550 cone and plate viscometer (PK1.1°) |
Gwent Electronic Materials C2021031D3 Electrode Ink Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |