Viscosity 18 cP
18 cP
D=30/s; DIN 54 453
3M Dyneon™ TF 5039 PTFE Dispersion  (discontinued **)
Used for coating glass fiber fabrics.Dyneon PTFE dispersions are aqueous dispersions developed for use in metal coating formulations and for application of impregnation and fabric coating applicatio..
Viscosity 18 cP
18 cP
LG Chemical LGflex EBNW Plasticizer
Features: Excellent Adhesion, Transparency, and Non-endocrine disrupterApplication: PVC Food Package WrapInformation provided by LG Chemical
Viscosity 18 cP
18 cP
Apparent
CIMBAR Suspengel™ 200 Plus High Purity Bentonite, Industrial Grade
Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co..