Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 17500 - 19500 cP | 17500 - 19500 cP | Uncured |
Atom Adhesives AA-BOND 2101 Epoxy Adhesive AA-BOND 2101 is a clear medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and el.. |