Polymer Property : Viscosity = 2.95e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2.95e+6 cP

@Temperature 160 °C
2.95e+6 cP

@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Lubrizol Advanced Materials PEARLBOND® 104 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 104.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a high thermoplasticity level...