Polymer Property : Viscosity = 2050 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1090 - 2050 cP
1090 - 2050 cP
25% Toluene Solution at 25°C; BAM 922
Kraton® D4158 K (O/E SBS) Radial Copolymer
Description: Kraton D4158 K is an oiled, radial copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form: Kraton D4158 KT - ..