Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 205000 cP @Temperature 190 °C |
205000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 5224 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, high ethylene copolymer, and FDA compliantFeatures: High viscosity and low crystallinityApplications: Component of modified .. |