Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 210 cP | 210 cP | |
Lord Adhesives 8400 Fast Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Viscosity | 210 cP | 210 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® G1643 M (SEBS) Linear Triblock Copolymer Description: Kraton G1643 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 20%. It is supplied from North America in the physical form ide.. |
|||
Viscosity | 210 - 350 cP | 210 - 350 cP | |
Solvay IGEPAL® CO 710 Surfactant Chemical Name: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHEDCAS: 68412-54-4 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CO-710 is an excellent prima.. |