Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 212400 cP @Shear Rate 3000 1/s, Temperature 191 °C |
212400 cP @Shear Rate 3000 1/s, Temperature 375 °F |
Melt Viscosity |
Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications. |