Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 219000 cP @Shear Rate 300 1/s, Temperature 190 °C |
219000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |