Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 223000 - 223000 cP @Temperature 204 - 204 °C |
223000 - 223000 cP @Temperature 399 - 399 °F |
Average value: 223000 cP Grade Count:1 |