Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 130 - 230 cP | 130 - 230 cP | |
Huntsman Euredur 46 Cycloaliphatic Amine Approx. H+ equivalent weight 95. Mix Ratio with GY 6010 is 50.Comments/Applications: Modified polyamine adduct for solvent free coatings, epoxy mortars, lower viscosity and higher chemical resista.. |
|||
Viscosity | 170 - 230 cP @Temperature 25.0 °C |
170 - 230 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT CR-30-20 MDI Isocyanate Description of product: Polymethylene-polyphenyl-isocyanate, 4,4-diphenyl-methane-diisocyanate (MDI) and mixture of its higher functionality, multi-ring oligomers.Field of application: With suitable.. |
|||
Viscosity | 170 - 230 cP @Temperature 25.0 °C |
170 - 230 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT CR30-20/LA MDI Isocyanate Description of product: Polymethylene-polyphenyl-isocyanate, 4,4`-diphenyl-methane-diisocyanate (MDI) and mixture of its higher functionality, multi-ring oligomers. Field of application: With suitab.. |