Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 23000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 23000 cP
23000 cP
Mixed (cp #52, 10 rpm)
Tra-Con Tra-Duct 921M01 Low Viscosity Long Pot Life Silver-Filled Epoxy
TRA-DUCT 921M01 is a two component, silver-filled electrically conductive epoxy adhesive designed for applications which require electrical conductivity and a long pot life at a relatively low heat ..
Viscosity 23000 cP
23000 cP
Hardener (cp #52, 10 rpm)
Tra-Con Tra-Bond 216R01 Fire Retardant Epoxy
TRA-BOND 216R01 is a fast curing material with a set time of 5 to 7 minutes. Samples tested were certified to the requirements of UL94 V-O, and is RoHS compliant. TRA-BOND 216R01 develops significa..
Viscosity 23000 cP
23000 cP
Dow Corning SYL-OFF® 7362 COATING
Syl-Off® 7362 Coating is a 30% solids dispersion of vinyl functional silicone polymer in toluene. A pre-catalysed coating suitable for fast cure applications, recommended for use with 7367 Crosslin..
Viscosity 23000 cP
23000 cP
Dynamic
Dow Corning SYL-OFF® PMCP7362 Coating
Syl-Off® 7362 Coating is a 30% solids dispersion of vinyl functional silicone polymer in toluene. A pre-catalysed coating suitable for fast cure applications, recommended for use with 7367 Crosslin..
Viscosity 23000 cP
23000 cP
Mixed
Armstrong A-5/A Epoxy Adhesive
Information provided by Ellsworth Adhesives.
Viscosity 23000 cP
23000 cP
Part A, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin
Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate ..