Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 18000 - 23000 cP | 18000 - 23000 cP | |
Huntsman Araldite HZ 340 Water-Based Hardener Base Resin is Polyamide. Typical Solids Content 50%. Approx. equivalent weight 113.Comments/Applications: Adhesives; Fiber-Sizing; Textiles; Abrasives; Paper treatment; Coatings Solvent free, good.. |
|||
Viscosity | 18000 - 23000 cP | 18000 - 23000 cP | |
Huntsman HZ 340 Polyamide Approx. H+ equivalent weight 113. Mix Ratio with GY 6010 is 120.Comments/Applications: Solvent free, water-based polyamide with good adhesion. For use in coatings for plaster, concrete, masonry, .. |
|||
Viscosity | 15000 - 23000 cP @Temperature 23.0 °C |
15000 - 23000 cP @Temperature 73.4 °F |
10 rpm |
Epoxy Technology EPO-TEK® H24 Electrically Conductive Epoxy Product Description: EPO-TEK® H24 is a two component, electrically and thermally conductive epoxy adhesive designed for semiconductor die attach and hybrid micro-electronics assembly.Advantages & A.. |