Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1200 - 2400 cP @Temperature 25.0 °C |
1200 - 2400 cP @Temperature 77.0 °F |
Uncured |
Permabond 268 Cyanoacrylate, General purpose PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano.. |
|||
Viscosity | 900 - 2400 cP | 900 - 2400 cP | |
Huntsman HY 3100 Aromatic Amine Approx. H+ equivalent weight 55. Mix Ratio with GY 6010 is 23.Comments/Applications: High solids coatings, floorings and tank linings. Good acetic acid resistance and other aggressive environment.. |
|||
Viscosity | 2200 - 2400 cP @Temperature 23.0 °C |
2200 - 2400 cP @Temperature 73.4 °F |
|
Master Bond MB297 Cyanoacrylate Adhesive System General purpose, fills gap to 0.008Information provided by Master Bond Inc. |
|||
Viscosity | 1800 - 2400 cP | 1800 - 2400 cP | NOV QC 020 |
Lubrizol ESTANE® 5735 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 1400 - 2400 cP @Temperature 23.0 °C |
1400 - 2400 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 360ST High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a slightly th.. |