Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 27 - 33 cP @Temperature 20.0 °C |
27 - 33 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 50-26 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 27 - 33 cP @Temperature 20.0 °C |
27 - 33 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 71-30 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 27 - 33 cP @Temperature 20.0 °C |
27 - 33 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 60-30 Polyvinyl Alcohol Intermediately Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 27 cP @Temperature 121 °C |
27 cP @Temperature 250 °F |
melt viscosity; ASTM D-3236 |
ExxonMobil Escorene® Escomer® H-101 Low MW HDPE Wax