Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2700 - 10000 cP | 2700 - 10000 cP | |
Huntsman HY 265 Cycloaliphatic Amine Approx. H+ equivalent weight 94. Mix Ratio with GY 6010 is 50.Comments/Applications: Modified cycloaliphatic polyamine adduct. Excellent chemical resistance. Exceptional sulfuric acid (96-98%) r.. |
|||
Viscosity | 2700 - 6400 cP | 2700 - 6400 cP | |
Huntsman HY 283 Cycloaliphatic Amine Approx. H+ equivalent weight 133. Mix Ratio with GY 6010 is 70.Comments/Applications: Modified polyamidoamine, low viscosity, solvent free. No induction, excellent gloss, chemical resistance. *F.. |
|||
Viscosity | 2700 - 3700 cP | 2700 - 3700 cP | |
Huntsman HY 837 Aliphatic Amine Approx. H+ equivalent weight 68. Mix Ratio with GY 6010 is 35.Comments/Applications: A medium viscosity liquid amine adduct. Fast cure, excellent adhesion, light color and outstanding chemical re.. |
|||
Viscosity | 2700 cP @Shear Rate 50.0 1/s, Temperature 240 °C |
2700 cP @Shear Rate 50.0 1/s, Temperature 464 °F |
Melt; ASTM D3835 |
Kureha KF Polymer 2950 PVDF Copolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Viscosity | 2700 cP @Temperature 177 °C |
2700 cP @Temperature 350 °F |
Typical |
Bostik 2109 Economical, low viscosity EVA Glue Stick Bostik 2109 Economical, low viscosity EVA Glue StickEconomical. Low viscosity for packaging applications. |