Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2849 cP @Temperature 23.0 °C |
2849 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® EV2118-2 Silver-filled, electrically conductive epoxy Preliminary Product Information SheetMaterial Description: A silver-filled, electrically conductive epoxy designed for semiconductor and electronic assembly.Information Provided by Epoxy Technology |