Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.00e+7 - 2.00e+8 cP @Temperature 316 - 316 °C |
3.00e+7 - 2.00e+8 cP @Temperature 601 - 601 °F |
Average value: 1.15e+8 cP Grade Count:2 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |