Viscosity | 2.90e+7 - 3.30e+7 cP | 2.90e+7 - 3.30e+7 cP | 232°C, 100 sec^-1; ASTM D3835 |
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Hylar 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and .. |