Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 312 cP | 312 cP | Dynamic |
Dow Corning 3580 Performance Modifier Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning |