Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 31300 cP @Shear Rate 11200 1/s, Temperature 200 °C |
31300 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |