Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 318500 cP | 318500 cP | Mixed, 2.5 rpm; TM R050-12 |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |