Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 320000 cP | 320000 cP | Melt Viscosity, 200°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Viscosity | 320000 cP | 320000 cP | Melt Viscosity, 200°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Viscosity | 320000 cP @Shear Rate 206 1/s, Temperature 200 °C |
320000 cP @Shear Rate 206 1/s, Temperature 392 °F |
ASTM D3835 |
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3190 can be processed by blow molding, injection molding or.. |