Physical Properties Metric English Comments
Viscosity 3360 cP
3360 cP
BASF Lupranate® 5070 Isocyanate
Description: Lupranate® 5070 Isocyanate is a low functional prepolymer based on pure MDI. Lupranate 5070 isocyanate is favored in solid elastomers and microcellular foams where the formulator desir..