Physical Properties Metric English Comments
Viscosity 34.5 cP
34.5 cP
Loctite® 294 High Temperature/Wicking Grade Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..