Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 374000 cP @Shear Rate 294 1/s, Temperature 190 °C |
374000 cP @Shear Rate 294 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys DuraGrip™ 6140 NC Thermoplastic Elastomer DuraGrip® 6140NC is an enhanced bonding and adhesion grade Thermoplastic Elastomer (TPE) designed for injection molding and extrusion processes. It will bond well with polycarbonate, polycarbonate .. |