Polymer Property : Viscosity = 4.1 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 4.1 cP
4.1 cP
Absolute
3M Fluorinert™ FC-40 Electronic Liquid
3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind..