Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4.4 cP @Temperature 25.0 °C |
4.4 cP @Temperature 77.0 °F |
|
LyondellBasell DPNP Dipropylene glycol normal propyl ether Information provided by Lyondell. |