Polymer Property : Viscosity = 4.57 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1.09 - 4.57 cP

@Temperature 190 - 230 °C
1.09 - 4.57 cP

@Temperature 374 - 446 °F
Average value: 1.29e+6 cP Grade Count:1
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..