Polymer Property : Viscosity = 42 cP
Polymer Property :
Viscosity =
42 cP
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Viscosity
32
-
42
cP
32
-
42
cP
Huntsman Araldite ECN 9511 Epoxy Cresol Novolac
Weight per Epoxide (EEW, g/eq) 200 to 227. Max color is