Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 600 - 4200 cP @Temperature 140 - 140 °C |
600 - 4200 cP @Temperature 284 - 284 °F |
Average value: 1.60e+6 cP Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Viscosity | 3600 - 4200 cP | 3600 - 4200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-626SH TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Viscosity | 100 - 4200 cP | 100 - 4200 cP | Milled Cement; Zeon Test #327 |
Zeon Chemicals Nipol® 1001CG Nitrile Elastomer Nipol 1001CG is a copolymer of butadiene and acrylonitrile of high oil resistance. Sufficient antioxidant has been added during manufacture for normal storage conditions.Excellent oil and fuel resis.. |
|||
Viscosity | 1000 - 4200 cP | 1000 - 4200 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1022 Nitrile Elastomer Nipol 1022 is a copolymer of butadiene and acrylonitrile with medium oil resistance and is directly soluble in many solvents without the necessity of mill breakdown. Sufficient nonstaining antioxida.. |
|||
Viscosity | 3500 - 4200 cP @Temperature 35.0 °C |
3500 - 4200 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 60 Polymeric Plasticizer Description: Formulated with PVC, it is used for the production of fuel pipes, solvents or other oil products.Information provided by P.A.T. Products, Inc. |