Polymer Property : Viscosity = 420000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 420000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
420000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer
DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent soft touch feel a..
Viscosity 420000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
420000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Advanced Polymer Alloys DuraGrip™ DGR 6170 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6170 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6, Nylon 6/6, glass filled Nylo..