Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 455000 cP @Shear Rate 300 1/s, Temperature 190 °C |
455000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 2180 NC Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |