Viscosity 22.0 - 47.0 cP
22.0 - 47.0 cP
Average value: 31.3 cP Grade Count:3
Overview of materials for Polytetrafluoroethylene (PTFE) Powder
This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..