Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 4800 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 4800 cP
4800 cP
Mixed (cp #52, 10 rpm)
Tra-Con Tra-Duct 926H01
Information provided by Tra-Con Inc.
Viscosity 4800 cP

@Temperature -10.0 °C
4800 cP

@Temperature 14.0 °F
Cold Crank
ChevronTexaco 600R Neutral Oil
FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o..
Copyright © lookpolymers.com All Rights Reserved