Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 485 cP @Temperature 40.0 °C |
485 cP @Temperature 104 °F |
25% in dimethylacetamide; Internal Method |
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
Viscosity | 485 cP | 485 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Viscosity | 485 cP @Temperature 30.0 °C |
485 cP @Temperature 86.0 °F |
|
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 250 System Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 250 system.Typical ApplicationsMulti-purpose modelsRTV mold patternsForm/Fit/.. |
|||
Viscosity | 485 cP @Temperature 30.0 °C |
485 cP @Temperature 86.0 °F |
|
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 500 System Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 500 system.All information provided by 3D Systems. |
|||
Viscosity | 485 cP @Temperature 30.0 °C |
485 cP @Temperature 86.0 °F |
|
3D Systems Accura® 40 Plastic for SLA® Systems 40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a.. |
|||
Viscosity | 485 cP @Temperature 30.0 °C |
485 cP @Temperature 86.0 °F |
|
3D Systems Accura® SI 40 Plastic for the SLA® 250 System Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |
|||
Viscosity | 485 cP @Temperature 30.0 °C |
485 cP @Temperature 86.0 °F |
|
3D Systems Accura® SI 40 Plastic for the SLA® 500 System Accura 40 "Ar" or "Hc" type materials - for the SLA 500 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |
|||
Viscosity | 485 cP @Temperature 30.0 °C |
485 cP @Temperature 86.0 °F |
|
3D Systems Accura® 10 Plastic for SLA® Systems Accura 10 "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsGeneral use prototyping for many uses, including:Enclosures, covers and casesCellular/mobile ph.. |