Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5.0 cP | 5.0 cP | |
Ritelok ECS Ethyl CA Adhesive Cyanoacrylate. Designed to penetrate by capillary action between pre-assembled components. High Strength, Low viscosity, Penetrating action |
|||
Viscosity | 5.0 cP | 5.0 cP | |
ND Industries 623 Heptane-Acetone SuperGlue accelerator Fast Acting SuperGlue accelerator, general purpose for porous surfaces or large gaps. Non-ozone depleting but flammable solvent |
|||
Viscosity | 5.0 - 15 cP | 5.0 - 15 cP | |
ND Industries SuperGlue Ethyl 320 Very low viscosity for pre-assembled componentsMeets military spec Mil-A-46050C Type II Class I |
|||
Viscosity | 5.0 cP | 5.0 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120 LOW ODER advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's p.. |
|||
Viscosity | >= 5.0 cP | >= 5.0 cP | ASTM D2196 |
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket Description: The Tecknit TECKSOF 2000 Series gasket consists of conductive fabric over foam and has been designed to meet today’s commercial EMI shielding applications demands where wide tolerance .. |
|||
Viscosity | >= 5.0 cP | >= 5.0 cP | ASTM D2196 |
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6101 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6001 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6801 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6802 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6901 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Viscosity | 5.0 - 25 cP | 5.0 - 25 cP | |
Huntsman Araldite DY 023 Reactive Diluent Weight per Epoxide (EEW, g/eq) 167 to 182. Max color is 1.Comments/Applications: Cresyl glycidyl ether - monofunctional epoxy. Less volatile and better resistance to water, but less efficient visc.. |
|||
Viscosity | 5.0 - 300 cP @Temperature 20.0 °C |
5.0 - 300 cP @Temperature 68.0 °F |
2%, Hoppler |
Mikro-Technik 8036 R/U Carboxymethylcellulose (CMC) Purified GradeComments: All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E). Reduced active contents down to 50 % are available. Special conce.. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
As Supplied |
Heraeus Cleviosâ„¢ P Jet N V2 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet N V2 is an antistatic material based on .. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
As Supplied |
Heraeus Cleviosâ„¢ P Jet UA Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet UA is an antistatic material based on PE.. |
|||
Viscosity | 5.0 - 12 cP | 5.0 - 12 cP | As Supplied |
Heraeus Cleviosâ„¢ P VP AI 4083 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP AI 4083 is an antistatic material based o.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Loctite® 408 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 5.0 - 15 cP | 5.0 - 15 cP | ASTM D445 |
ExxonMobil Jayflex™ MB10 Plasticizer Availability: AmericasCAS Number: 131298-44-7EINECS Number: 421-090-1Information provided by ExxonMobil |
|||
Viscosity | 5.0 - 15 cP | 5.0 - 15 cP | ASTM D445 |
ExxonMobil Jayflex™ MB10 Plasticizer (European Grade) Availability: Europe, Middle East & AfricaCAS Number: 131298-44-7EINECS Number: 421-090-1Information provided by ExxonMobil |
|||
Viscosity | 5.0 cP @Temperature 43.0 °C |
5.0 cP @Temperature 109 °F |
|
Dow ISONATE™ 125MDR Pure MDI ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers .. |
|||
Viscosity | <= 5.0 cP | <= 5.0 cP | |
3M Scotch-Weld™ AC68 Instant Adhesive Debonder 3M™ Scotch-Weld™ Instant Adhesive Debonder AC68 attacks and dissolves cured instant adhesives. It is formulated to have a relatively low evaporation rate and can be used to debond misaligned parts.. |
|||
Viscosity | <= 5.0 cP | <= 5.0 cP | |
3M Scotch-Weld™ AC79 Instant Adhesive Primer 3M™ Scotch-Weld™ Instant Adhesive Primer AC79 is a California compliant version of AC78.Information provided by 3M |
|||
Viscosity | 5.0 - 30 cP | 5.0 - 30 cP | @ 275 |
ACC 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion 1KSP is a silicone modified polyurea dispersion “Powered by ReactAmine® Technology” designed for a wide range of rigid and flexible substrates such as wood, metal, vinyl, concrete and other plast.. |
|||
Viscosity | 5.0 cP @Temperature 25.0 °C |
5.0 cP @Temperature 77.0 °F |
|
Parker Chomerics CHO-SHIELD® 1085 Silicone Adhesive Primer Air-drying liquid coatings used to improve the adhesion of Chomerics CHO-BOND conductive silicone elastomers to metal and other non-silicone substrates. The primers are moisture reactive and clear i.. |
|||
Viscosity | 5.0 cP @Temperature 25.0 °C |
5.0 cP @Temperature 77.0 °F |
|
Parker Chomerics CHO-SHIELD® 1086 Silicone Adhesive Primer Air-drying liquid coatings used to improve the adhesion of Chomerics CHO-BOND conductive silicone elastomers to metal and other non-silicone substrates. The primers are moisture reactive and clear i.. |
|||
Viscosity | 5.0 cP @Temperature 25.0 °C |
5.0 cP @Temperature 77.0 °F |
|
Parker Chomerics CHO-SHIELD® 1091 PRIMER CHO-SHIELD 1091 is an air-drying liquid coating for enhancing the adhesion of CHO-SHIELD 2001 and 2003 corrosion resistant, electrically conductive coatings to chemically treated aluminum. CHO-SHIEL.. |
|||
Viscosity | 5.0 - 100 cP | 5.0 - 100 cP | #1 SP @ 60 rpm; RPG-0659 |
Solvay RHODISOLV® INFINITY Solvent Description: Rhodiasolv INFINITY is a blend of dibasic ester solvent and proprietary surfactantsChemical Name: Microemulsion concentrate based on dimethyl-2-methyl glutarateSolubility in water: 100%.. |