Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4400 - 5200 cP @Temperature 35.0 °C |
4400 - 5200 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G201 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 4400 - 5200 cP @Temperature 35.0 °C |
4400 - 5200 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G210 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 4400 - 5200 cP @Temperature 35.0 °C |
4400 - 5200 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G202 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |