Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 525000 cP @Temperature 400 °C |
525000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Viscosity | 525000 cP @Temperature 400 °C |
525000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Viscosity | 525000 cP | 525000 cP | Melt Viscosity, 250°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific) NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C |
|||
Viscosity | 525000 cP @Temperature 400 °C |
525000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |