Polymer Property : Viscosity = 550000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 550000 cP
550000 cP
Ritelok PS67 Adhesive
Anaerobic. Pipe sealant, standard and stainless pipes. PS67 withstands temperatures from 65°F to 400°F (55°C-200°C), dismantled using normal tools
Viscosity 550000 cP

@Temperature 400 °C
550000 cP

@Temperature 752 °F
melt; ISO 11443
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Viscosity 550000 cP

@Temperature 400 °C
550000 cP

@Temperature 752 °F
ISO 11443
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Viscosity 550000 cP

@Temperature 400 °C
550000 cP

@Temperature 752 °F
Melt; ISO 11443
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Viscosity 550000 cP

@Shear Rate 190 1/s,
Temperature 230 °C
550000 cP

@Shear Rate 190 1/s,
Temperature 446 °F
Noltex Soarnol® ET3808 Ethylene Vinyl Alcohol Copolymer
Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
Viscosity 550000 cP

@Temperature 180 °C
550000 cP

@Temperature 356 °F
Melt; Flowtester (100 kgf/cm², dimension of die 1 Φ mm x 10 mm)
Zeon Chemicals Quintac® 3421 SIS Block Polymer
Styrene Isoprene (SIS) Block Polymer. Standard grade for hot melt PSAInformation provided by Zeon Chemicals L.P.
Viscosity 550000 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
550000 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity
Viscosity 550000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
550000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Advanced Polymer Alloys Alcryn® 2090 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Viscosity 550000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
550000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Advanced Polymer Alloys Alcryn® 2090 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Viscosity 550000 cP
550000 cP
Part B, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..