Physical Properties Metric English Comments
Viscosity 660 cP

@Temperature 121 °C
660 cP

@Temperature 250 °F
melt viscosity; ASTM D-3236
ExxonMobil Escorene® UL-7720 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
Viscosity 660 cP
660 cP
Von Roll Isola IMI Varnish 3405 Polyester Varnish for Electrical Insulation
Data provided by Von Roll Isola USA.Flash Point: