Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 675000 cP @Temperature 400 °C |
675000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |